Inconel and other nickel alloys, sorted by what they are built to survive
Nickel alloys split into two working families. Heat alloys keep their strength when hot. Corrosion alloys resist acids, chlorides and sour gas. Some do both. The table lists each alloy by its common designation and UNS number, the service it is built for and how hard it is to machine.
Nickel alloys by designation and UNS number
Machining effort is typical, against 316 stainless. Condition is the state a part is usually machined in. Your drawing and its specification always govern.
| Alloy | UNS | Family | Built for | Usually machined | Machining effort |
|---|---|---|---|---|---|
| Alloy 718 | N07718 | Heat | Strength up to about 650°C (1200°F), sour well parts | Solution treated, or solution treated and aged | Very high |
| Alloy X-750 | N07750 | Heat | Springs, bolts and seals that hold load when hot | Solution treated, or equalized and aged | High |
| Waspaloy | N07001 | Heat | Load-bearing parts from about 650 to 870°C (1200 to 1600°F) | Solution treated, stabilized and aged | Very high |
| Alloy X | N06002 | Heat | Combustor and duct parts, oxidation up to about 1200°C (2200°F) | Solution annealed | High |
| Alloy 625 | N06625 | Heat and corrosion | Seawater, chlorides, oxidation up to about 980°C (1800°F) | Annealed | High |
| Alloy 600 | N06600 | Heat and corrosion | Hot caustic, chlorine gas, furnace fixtures | Annealed | Moderate |
| Alloy C-276 | N10276 | Corrosion | Reducing acids, wet chlorine, severe sour gas | Solution annealed | Very high |
| Alloy 825 | N08825 | Corrosion | Sulfuric and phosphoric acid at a lower material cost | Annealed | Moderate |
| Alloy 925 | N09925 | Corrosion | Oil tools and hangers in sour wells | Aged | High |
| Alloy 400 | N04400 | Corrosion | Flowing seawater, hydrofluoric acid, alkalis | Annealed or cold drawn and stress relieved | Moderate |
| Alloy K-500 | N05500 | Corrosion | Seawater parts that need two to three times the strength of 400 | Annealed, or aged after rough machining | High |
Heat alloys
Strengthened by fine particles that form during an aging treatment, or by heavy alloying. They hold load and resist creep where stainless steel softens. The same strength makes them abrasive and slow to cut, and the aging step has to be placed in the machining plan.
Alloy 600, Alloy 625, Alloy 718, Alloy X-750, Waspaloy, Alloy X.
Corrosion alloys
High nickel with chromium, molybdenum, copper or tungsten. The chemistry is chosen for the medium: seawater, reducing or oxidizing acids, hydrofluoric acid or sour gas. They are tough and work harden quickly, so sharp tools and steady cuts matter more than raw machine power.
Alloy 400, Alloy 600, Alloy 625, Alloy 825, Alloy 925, Alloy C-276, Alloy K-500.
Alloy detail pages
What the alloy is, how it machines, where it is used, the specifications that usually appear on drawings, typical tolerances and what to write on the RFQ.
Alloy 718
Age-hardened strength up to about 650°C (1200°F) and the common choice for sour well parts.
Alloy 625
Seawater, hot chlorides and oxidation, with no aging step in the machining plan.
Alloy C-276
Reducing acids, wet chlorine and severe sour gas. Among the slowest to machine.
Alloy 400
Nickel-copper for flowing seawater and hydrofluoric acid. The easiest of the family to cut.
Trade names and designations
Drawings and specifications name these alloys in different ways: a trade name, a common number such as 718, a UNS number such as N07718 or a werkstoff number such as 2.4668. Any of them works on the RFQ. The quote names the alloy by its specification and UNS number, so it reads the same whichever name your drawing uses.
Inconel, Monel, Hastelloy and other alloy names are trademarks of their respective owners. This site is not affiliated with them.