Alloys / Alloy 400
Alloy 400, UNS N04400Alloy 400 machining for seawater and hydrofluoric acid
Alloy 400 is the nickel-copper alloy with the longest record in flowing seawater and hydrofluoric acid service. It is also the easiest alloy of the family to machine, which makes it the lower-cost answer for many marine and chemical parts. This page covers its limits, its machining and its stronger relative K-500.
- UNSN04400
- TypeNickel-copper
- FamilyCorrosion
- Built forFlowing seawater, hydrofluoric acid, alkalis
- MachinedAnnealed or cold drawn and stress relieved
- EffortModerate, typical against 316 stainless
What Alloy 400 is
Alloy 400 is about two thirds nickel and one third copper. It resists flowing seawater, brackish water, hydrofluoric acid, alkalis and many non-oxidizing acids. It is weaker in oxidizing acids and can pit in stagnant seawater, under deposits and in tight crevices.
Its strength comes from cold work, not from heat treatment. Where a part needs more strength with the same corrosion behavior, alloy K-500 (UNS N05500) adds aluminum and titanium and is age hardened to roughly two to three times the yield strength of annealed 400.
How Alloy 400 machines
Annealed 400 is soft and gummy, which tears the surface and builds up on the tool edge. Cold-drawn, stress-relieved bar cuts cleaner and is the usual choice for turned parts. Cutting speeds are higher than in 625 or 718, so cycle times are shorter.
A free-machining version, alloy R-405 (UNS N04405), adds sulfur for long production runs of turned parts. The sulfur lowers corrosion resistance a little and hurts weldability, so it is only used when the drawing allows it.
- ConditionCold drawn and stress relieved for turned parts. Annealed when the part is formed or welded.
- ToolsSharp edges and positive rake to stop tearing and built-up edge.
- K-500Rough in the annealed condition, age, then finish the critical features.
- MagnetismAlloy 400 is slightly magnetic near room temperature. Use K-500 where low permeability is specified.
Where Alloy 400 parts are used
Marine
Seawater pump and valve parts, fasteners, propeller and pump shafts (often K-500).
Chemical and refining
Valve trim, fittings and pump parts in hydrofluoric acid alkylation and caustic service.
Water and brine
Brine heater parts, desalination fittings and feedwater hardware.
Instruments
Gauge parts, springs and housings where corrosion resistance and stable dimensions matter.
Specifications often seen on drawings
For reference only. Material is bought to the specification on your drawing, and the mill certificate shows it.
- ASTM B164Rod, bar and wire, including the free-machining alloy R-405.
- ASTM B127Plate, sheet and strip.
- ASTM B564Forgings.
- QQ-N-281Federal specification still cited on older drawings.
Typical tolerances and finishes
Typical ranges for well-designed nickel alloy parts, not promises. The quote confirms what can be held on your geometry, feature by feature.
Alloy 400 holds the tight end of these ranges more easily than the heat alloys. Aged K-500 behaves more like 718 and is finished after aging where tolerances are tight.
| Feature | Typical |
|---|---|
| General milled and turned features | ±0.005 in (±0.13 mm) |
| Precision features, bores and fits | ±0.001 in (±0.025 mm) |
| Ground or finish-machined features | ±0.0003 to ±0.0005 in (±0.008 to ±0.013 mm) |
| Surface finish, machined | 63 to 32 µin Ra (1.6 to 0.8 µm) |
| Surface finish, ground | 16 µin Ra (0.4 µm) or finer |
- As machinedThe usual state for 400 parts.
- PolishedFor sealing faces and valve stems.
- Pickled or cleanedWhen the drawing calls for a clean surface before service.
- Penetrant testWhen the drawing calls for it.
What to put on the drawing or RFQ
Each line removes a question from the drawing review and a guess from the quote.
Related alloys: Alloy 625, Alloy C-276, Alloy 718. Heat treatment and machining sequence.
- Alloy 400, R-405 or K-500, and whether R-405 is allowed as a substitute.
- The specification and condition, for example ASTM B164, cold drawn and stress relieved.
- Aged hardness for K-500 parts and where it is measured.
- Magnetic permeability limits, if any.
- Whether the part will see stagnant seawater, so the alloy can be checked before pricing.
Quote your Alloy 400 part
Send the drawing with quantity and the specification. We reply within 24 business hours with questions or a feasibility note, then one itemised quote for the finished parts. The full RFQ form takes condition, service temperature and the documents you need.
Inconel, Monel, Hastelloy and other alloy names are trademarks of their respective owners. This site is not affiliated with them.