Skip to content

Alloys / Alloy 718

Alloy 718, UNS N07718

Alloy 718 machining for parts that carry load when hot

Alloy 718 is the nickel alloy most drawings ask for when a part must stay strong up to about 650°C (1200°F) or survive a sour well. It is also one of the slowest to machine once aged. This page covers what changes the time and cost of a 718 part and what to put on the drawing so the quote is right the first time.

  • UNSN07718
  • TypeAge-hardened Ni-Cr-Fe with niobium
  • FamilyHeat
  • Built forStrength up to about 650°C (1200°F), sour well parts
  • MachinedSolution treated, or solution treated and aged
  • EffortVery high, typical against 316 stainless

What Alloy 718 is

Alloy 718 is a nickel-chromium-iron alloy strengthened by niobium and some titanium and aluminum. After an aging treatment, fine gamma double-prime particles form in the metal and give it high yield strength that holds up to about 650°C (1200°F). Above that, the particles coarsen and strength falls quickly.

The alloy ages slowly, which is why it welds better than most age-hardened nickel alloys. That same slow response gives the machining plan a choice: cut the part in the solution-treated condition and age it afterwards, or cut it fully aged.

How Alloy 718 machines

Aged 718 typically sits in the high 30s to mid 40s HRC and is abrasive. Tools wear at the depth-of-cut line, heat stays in the cutting zone and the metal work hardens under a dull edge. Cutting speeds are a fraction of those used on stainless steel, so cycle time and tooling drive the price.

Solution-treated 718 is softer and cuts faster, but the part shrinks slightly and can move when it is aged afterwards. Where tolerances are tight, the usual route is to rough in the solution-treated condition, age, then finish-machine the critical features.

  • RoughingHigh-pressure coolant, a varied depth of cut to spread notch wear and no dwelling in the cut.
  • Holes and threadsSmall deep holes and small taps are the costliest features. Thread milling is often safer than tapping in aged material.
  • Thin wallsResidual stress from bar or forging can move a thin part. A stress relief or a balanced roughing plan keeps it in tolerance.
  • Finish passesTaken after aging on the features that carry the tightest tolerances and the surface finish callouts.

Where Alloy 718 parts are used

Oil and gas

Wellhead and valve parts, hangers, downhole tool bodies and fasteners, usually to API 6ACRA and NACE MR0175 / ISO 15156.

Power and turbines

Rings, seals, casings, shafts and bolts for gas and steam turbines.

Aerospace ground hardware

Test cell fixtures, high-temperature tooling and test stand parts.

Industrial

Springs, fasteners and pump parts that need strength with corrosion resistance.

Specifications often seen on drawings

For reference only. Material is bought to the specification on your drawing, and the mill certificate shows it.

  • AMS 5662Bars, forgings and rings, solution heat treated.
  • AMS 5663Bars, forgings and rings, solution and precipitation heat treated.
  • AMS 5596Sheet, strip and plate.
  • ASTM B637Bars, forgings and forging stock for age-hardened nickel alloys.
  • API 6ACRAAge-hardened nickel alloys for oil and gas drilling and production equipment.

Typical tolerances and finishes

Typical ranges for well-designed nickel alloy parts, not promises. The quote confirms what can be held on your geometry, feature by feature.

Features finished after aging hold the tight end of these ranges. Features cut before aging carry the movement of the aging step.

FeatureTypical
General milled and turned features±0.005 in (±0.13 mm)
Precision features, bores and fits±0.001 in (±0.025 mm)
Ground or finish-machined features±0.0003 to ±0.0005 in (±0.008 to ±0.013 mm)
Surface finish, machined63 to 32 µin Ra (1.6 to 0.8 µm)
Surface finish, ground16 µin Ra (0.4 µm) or finer
  • As machinedThe usual state for 718 parts.
  • Ground or lappedFor seal faces, bearing fits and fine surface finish callouts.
  • Bead blastFor a uniform matte surface, with masking of critical features.
  • Penetrant testWhen the drawing calls for it, done after the final machining step.

What to put on the drawing or RFQ

Each line removes a question from the drawing review and a guess from the quote.

Related alloys: Alloy 625, Alloy X-750, Waspaloy. Heat treatment and machining sequence.

  • The material specification and the condition at delivery, for example AMS 5663 or API 6ACRA.
  • The hardness requirement and where on the part it is measured.
  • Whether aging may be done after rough machining, or the part must be cut from aged stock.
  • NACE MR0175 / ISO 15156 edition and limits, if the part is for sour service.
  • Any penetrant test, first article report or material identification you need.

Quote your Alloy 718 part

Send the drawing with quantity and the specification. We reply within 24 business hours with questions or a feasibility note, then one itemised quote for the finished parts. The full RFQ form takes condition, service temperature and the documents you need.

Inconel, Monel, Hastelloy and other alloy names are trademarks of their respective owners. This site is not affiliated with them.

STEP, IGES, PDF, DWG, DXF or ZIP. No upload from this device: email the files to after you send this form.