Heat treatment of nickel alloys and where machining fits

For age-hardened alloys such as 718, the order of machining and heat treatment decides cutting time, tool cost and whether tight features stay in tolerance. This page explains the treatments in general terms. Your specification sets the actual cycle.

Three treatments, three jobs

Solution treatment

Heats the alloy high enough to dissolve the strengthening phases, then cools it fast. The result is a softer, uniform structure that machines and forms more easily and is ready to age.

Aging

Also called precipitation hardening. One or more holds at a lower temperature grow fine particles that give the alloy its strength and hardness. Only the age-hardenable alloys respond.

Stress relief

A lower-temperature hold that relaxes residual stress from bar production, welding or heavy roughing. Used to keep thin or long parts from moving during later steps.

Typical aging cycles

Typical published cycles, rounded, for general information. They are not instructions. The specification on your drawing sets the temperatures, times, cooling and hardness range, and the heat treatment certificate shows what was done.

AlloyBefore agingAging, typicalNote
Alloy 718Solution treat about 925 to 1010°C (1700 to 1850°F)About 718°C (1325°F) for 8 h, furnace cool to about 621°C (1150°F), hold to about 18 h in total, air coolThe two-step age is the common AMS 5663 style cycle. Some oil and gas specs use other cycles.
Alloy X-750Solution treat, or an equalizing step of about 885°C (1625°F) for 24 hAbout 704°C (1300°F) for 20 hSpring and bolt specs choose between several cycles for strength or relaxation resistance.
WaspaloySolution treat about 995 to 1040°C (1825 to 1900°F)Stabilize about 845°C (1550°F) for 4 h, then age about 760°C (1400°F) for 16 hThree steps. Rotating and static parts can carry different cycles.
Alloy K-500Anneal when needed for forming or before rough machiningAbout 590 to 610°C (1100°F) for around 16 h, then slow cool to about 480°C (900°F)Cold-worked material ages to higher hardness than annealed material.
Alloy 925Solution treat per the oil and gas specificationAbout 740°C (1365°F) for 8 h, furnace cool to about 620°C (1150°F) and holdAPI 6ACRA and customer specs set the cycle and the hardness range.

Alloys that are not age hardened

Several common nickel alloys get their strength from their chemistry or from cold work, not from aging. For these, the machining plan has no hardening step to work around, which is one reason 625 is often quicker to hold tolerance on than aged 718.

  • Alloy 625Supplied annealed. Not hardened by an aging treatment. A stress relief may be specified for welded or heavily machined parts.
  • Alloy C-276Used solution annealed, with a rapid quench from about 1120°C (2050°F). Cannot be hardened by heat treatment.
  • Alloy 400Annealed or cold worked. Strength comes from cold work, which a stress relief keeps while lowering residual stress.
  • Alloy 600 and alloy XAnnealed or solution annealed. Used in that condition for heat and corrosion service.

Sequencing machining and heat treatment

For an age-hardened part there are three usual routes. The drawing review picks one with you, and the quote prices that route. If your specification fixes the route, say so on the RFQ.

  1. Machine fully aged stock

    The part is cut from material already aged to the spec. No movement from heat treatment afterwards, but the slowest cutting and the highest tool cost. Common for small parts and tight tolerances.

  2. Rough, age, finish

    Rough in the solution-treated condition, age, then finish the critical features. Faster cutting for most of the stock and full control of the final size. The most common route for larger 718 parts.

  3. Machine, then age

    Machine the whole part soft and age it last. Fastest cutting, but the part shrinks slightly and can distort. Fits parts with open tolerances and no thin walls.

What to write on the drawing

Heat treatment gaps are the most common reason a nickel alloy RFQ comes back with questions.

  • The material specification and the condition at delivery, for example AMS 5663 or API 6ACRA.
  • The hardness or strength requirement, the scale and where on the part it is measured.
  • Whether heat treatment may be done after rough machining.
  • Any furnace or pyrometry standard and any accreditation the heat treater must hold.
  • Test coupons or tensile tests, if the specification calls for them.

Heat treatment questions

Related: Alloy 718, quality and documents.

Does alloy 718 change size when it is aged?

Yes. Aging causes a small, predictable contraction and can release residual stress from the bar or forging. On loose features it does not matter. On tight bores, fits and thin walls, the usual answer is to finish-machine those features after aging.

Who arranges the heat treatment?

It is part of the order. The heat treatment is done by a heat treater suited to the alloy and the specification, and its certificate and hardness results come with the parts. If your drawing names an accreditation or a pyrometry standard for the furnace, write it on the RFQ and the quote states how it is met.

Can a part be re-aged if the hardness is wrong?

Sometimes, depending on the alloy and the specification. An under-aged 718 part can often be aged further. An over-aged part usually needs a new solution treatment and a full age, which can move the part. That is why hardness is checked before final machining where the sequence allows it.